RFID accessory NFC sticker EMC material on smart phone
License security solution license check with encryption algorithm
NFC quality inspect sticker like spirit ,alcohol,liquor bottle seal
Anti metal surface NFC tamper check on open tag
Serial NO printable on metal use rfid tag
Increased improvement of mobile NFC system;
Production can flesible;
Increased magnetic field convergence by relative magnetic permeability
Type:Ferrite sheet
Effective carrier frequency:13.56MHZ and below
Operating temperature(.C):-30.C to +85.C
Permeability(@13.56MHZ) ̡:43.2395
Surface resistivity():>=108R
Heat conductivity(W/m.k):1.0 W/m.k
胶带:定制可选的
Color:Black
Test device :HP4285A;
The information and statements here are believed to be reliable but are not to be construed as a warranty or representation for which we assume legal responsibility.
Users should undertake sufficient verification and testing to determine the suitability for their own particular purpose of any information or products referred to herein.
Item code | Dimenssion(mm) | Cover thickness(mm) | 胶厚度(毫米) | Total thickness(mm) | Tolerance(mm) |
---|---|---|---|---|---|
IVF-N012-A1T-300x200 | Roll maximum 250mmx20m or sheet customilzed | customilzed | 0.015/ 0.03 | 0.12 | 0.01 |
IVF-N023-A2T-300x200 | Roll maximum 250mmx20m or sheet customilzed | customilzed | 0.015/ 0.03 | 0.23 | 0.01 |
IVF-N030-A2T-300x200 | Roll maximum 250mmx20m or sheet customilzed | customilzed | 0.015/ 0.03 | 0.3 | 0.01 |
IVF-N045-A2T-300x200 | Roll maximum 250mmx20m or sheet customilzed | customilzed | 0.015/ 0.03 | 0.45 | 0.01 |
IVF-N060-A2T-300x200 | Roll maximum 250mmx20m or sheet customilzed | customilzed | 0.015/ 0.03 | 0.60 | 0.01 |
No. | ITEM | TEST CONDITION | TEST REQUIREMENTS |
---|---|---|---|
1 | High Temperature Resistance | 1. Temperature : +85 5 2. Time : 96 hrs 3. Measure after left for 60 min. at room |
1. No visual damage 2. Permeability change within 15% |
2 | Low Temperature Resistance | 1. Temperature : -40 5 2. Time : 96 hrs 3. Measure after left for 60 min. t room |
1. No visual damage 2. Permeability change within 15% |
3 | Humidity(Steady Condition) | 1. Humidity : 80 % RH 2. Temperature : +80 3 3. Time : 120 hrs 4. Measure after left for 60 min. at room |
1. No visual damage 2. Permeability change within 15% |
The information and statements here are believed to be reliable but are not to be construed as a warranty or representation for which we assume legal responsibility.
Exclusive Design & Patent Technology
Factory Quality Service
Support OEM, ODM & SKD services,acccept from the processing of Etching, Flip-chip Assembly, Lamination, Die-cut, Program Encoding ( TID/UID, Serial Number, Barcode , Associated All of the related Datas )
Free Samples Provided existing in warehouse
Good Price & competitively
根据要求定制uirement
Customized Antennna,Inlay,Label Design to Required System
Confidential Security Product Structure Design & Evaluation
Free Charge Analysis & Simulate Performance Character
Free Charge Solution Consulting Including fine Tuning
Free Provide Workflow of Tag , Inlay and Antenna production
Free Charge User Manual Instruction To Special Requirement
Payment Term: T/T, Western Union & Paypal.
Quick customized sample providing of 3-7 days, low cost.
Packaging Defined of your needs, Normally supply is in roll by roll with 2000-5000 pcs roll/bag & Paper Carton. Some specified tag can be supplied in piece by piece with 50-200tags per small bag/carton.
Shipping Method & Delivery Time: Fastest 8-12 business days by DHL,UPS,FedEx,EMS and so on couriers or sea-cargo air-cargo appointed from the customer.